Atomic layer deposition of amorphous TiO2 on graphene as an anode for Li-ion batteries

Chunmei Ban, Ming Xie, Xiang Sun, Jonathan J. Travis, Gongkai Wang, Hongtao Sun, Anne C. Dillon, Jie Lian, Steven M. George

Research output: Contribution to journalArticlepeer-review

82 Scopus citations

Fingerprint

Dive into the research topics of 'Atomic layer deposition of amorphous TiO2 on graphene as an anode for Li-ion batteries'. Together they form a unique fingerprint.

Engineering & Materials Science

Chemical Compounds